Tensile Strength: 71,000 PSI (490 MPa) Yield Strength: 60,000 PSI (415 MPa) Elongation: 25% Conductivity: 14.3 Density: 9.59/cm Hardness: Brinell 130
After cleaning metal, preheat generally to 176 deg C then heat the joint area to 426 deg C. Melt off some flux and allow it to flow throughout the joint. Then add alloy.