Recommended Current: DC Reverse (+) or AC
Deposition Rates:
Diameter
Length
Weldmetal/ Electrode
Arc Time of Deposition min/ lb
Amperage Settings
3/32"
12"
.44 oz
45
70
1/8"
14"
.76 oz
22
90
5/32"
1.07 oz
20
120
Tensile Strength: 76,000 psi (525 MPa)
Yield Strength: 53,000 psi (370 MPa)
Elongation: 29%
Hardness: Rockwell B 87-90, Brinell 179 Vickers 197
Welding Techniques: Guide the electrode at a steep angle keeping the arc length short. Use short staggered beads when welding restrained parts.
Welding Positions: Flat, Vertical up, Horizontal, Overhead